@article{Sagrera-Moreno_González-Vila_Aguanell-García_Gaspar-Tebar_1990, title={Durabilidad del hormigón: Acción de disoluciones de sulfato de calcio y de sulfato de magnesio sobre un cemento Portland de alta resistencia inicial. Influencia de la adición de escorias y de cenizas volantes}, volume={40}, url={https://materconstrucc.revistas.csic.es/index.php/materconstrucc/article/view/771}, DOI={10.3989/mc.1990.v40.i219.771}, abstractNote={This article —included on a long time ICCET Investigation Program— studies the mechanical resistances variation, to flexure, of the 1 X 1 X 6 cm mortar samples (1:3) made with high initial resistance cement and with several slags addition (cement/slag = 85/15 - 65/35 - 40/60 and 30/70) with high furnace slag and a fly ash (with selected characteristies) when they were submited after the cured period (1 day at 100% R.H. and 21 days inside filtered potable water) to the action of the gypsum saturated solution, four magnesium sulphate solutions with the next concentrations (3.22 - 32.20 - 128.80 and 515.20 g/l of MgS0<sub>4</sub>4.7H<sub>2</sub>0), gypsum saturated solution with 3.22 g/l MgS0<sub>4</sub>.7H<sub>2</sub>0 a gypsum saturated solution with 32.20 g/l MgSO<sub>4</sub>. 7H<sub>2</sub>O and, moreover, filtered potable water, during 56-90-180- 360 - 540 - 720 - 900 and 1080 days. The results obtained have produced a clasification accord to the mechanical behaviour to flexure of the cement n. ° 1 and the mixed cement n.° 1/slag and cement n.° 1/fly ash, front to the agressive solutions mentioned.}, number={219}, journal={Materiales de Construcción}, author={Sagrera-Moreno, José Luis and González-Vila, Victoriano and Aguanell-García, Manuel and Gaspar-Tebar, Demetrio}, year={1990}, month={Sep.}, pages={49–66} }