Experimental evaluation of the effect of different design conditions on the risk of decay in solid wood exposed to outdoor climate
DOI:
https://doi.org/10.3989/mc.2021.12220Keywords:
Wood, Decay, Durability, Moisture content, Long-term behaviourAbstract
Wood decay have the greatest impact on in-service wood structural elements. In most cases, decay is associated with excessive accumulation of moisture in the wood. The structural design conditions have an effect on the wood moisture content and this affects the service life of the material. In this study, which involved an experimental trial specifically designed to embrace different structural design conditions, the moisture content evolution in different places affected by different design conditions was evaluated over a period of three years in Madrid (Spain). The effect of protection by eaves, separation from the ground and the vertical or horizontal arrangement of the wood elements on the monthly evolution of the moisture content and decay risk are assessed.
Downloads
References
Brischke, C.; Jones, D. (2016) Performance of bio-based building products - Recent activities within COST Action FP 1303, Holztechnologie. 57 [2], 47-54.
Brischke, C.; Bayerbach, R.; Rapp, A.O. (2007) Decay influencing factors: a basis for service life prediction of wood and wood-based products. Wood Mat. Sci. Eng. 1, 91-107. https://doi.org/10.1080/17480270601019658
Brischke, C.; Soetbeer, A.; Meyer-Veltrup, L. (2017) The minimum moisture threshold for wood decay by basidiomycetes revisited. A review and modified pile experiments with Norway spruce and European beech decayed by Coniophora puteana and Trametes versicolor. Holzforschung. 71 [11], 893-903. https://doi.org/10.1515/hf-2017-0051
Morris, P.; Winandy, J.E. (2002) Limiting conditions for decay in wood systems. International Research Group on Wood Protection, Stockholm, IRG/WP 02-10421.
Isaksson, T.; Thelandersson, S. (2013) Experimental investigation on the effect of detail design on wood moisture content in outdoor above ground applications. Build. Environ. 59, 239-249. https://doi.org/10.1016/j.buildenv.2012.08.023
Meyer-Veltrup, L.; Brischke, C. (2017) Design and performance prediction of timber structures based on a factorization approach. International Research Group on Wood Protection, Stockholm,IRG/WP 17-20603. IRG, Stockholm.
Brischke, C.; Thelandersson, S. (2014) Modelling the outdoor performance of wood products - A review on existing approaches. Const. Buil. Mater. 66, 384-397. https://doi.org/10.1016/j.conbuildmat.2014.05.087
Thelandersson, S.; Isaksson, T.; Suttie, E.; Frühwald, E.; Toratti, T.; Grüll, G.; Viitanen, H.; Jermer, J. (2011) Service life of wood in outdoor above ground applications: Engineering design guideline. Background document. Rapport TVBK-3061, ISSN 0349-4969. Lund University, Sweden.
Isaksson, T.; Thelandersson, S.; Jermer, J.; Brischke, C. (2015) Service life of wood in outdoor above ground applications: Engineering design guideline. Background document Rapport TVBK-3067. Lund University, Division of Structural Engineering, Lund, Sweden. ISBN 978-87993-02-2.
Jermer, J. (Editor); Thelandersson, S.; Viitanen, H.; Toratti, T.; Grüll, G.; Steitz, A.; Michael, T.; Bader, T.; Alfredsen, G.; Suttie, E.; De Windt, I.; Van Acker, J.; Bollmus, S.; Podgorski, L. (2011) WoodExter-Service life and performance of exterior wood above ground. Final SP Report 2011: 53 pp.
UNE-EN 252:2015 Field test method for determining the relative protective effectiveness of a wood preservative in ground contact. AENOR, Asociación Española de Normalización (in Spanish).
ISO 15686-1 (2011) Buildings and constructed assets - Service life planning - Part 1: General principles and framework. International Organization for Standardization, Genève.
Marteinsson, B. (2003) Durability and the factor method of ISO 15686-1. Build. Res. Inf. 31 [6], 416-426. https://doi.org/10.1080/0961321032000105412
Fernandez-Golfin, J.; Larrumbide, E.; Ruano, A.; Galvan, J.; Conde, M. (2016) Wood decay hazard in Spain using the Scheffer index: proposal for an improvement. Eur. Wood Wood Prod. 74, 591-599. https://doi.org/10.1007/s00107-016-1036-z
Viitanen, H.; Toratti, T.; Peuhkuri, R.; Ojanen, T.; Makkonen, L. (2009) Evaluation of exposure conditions for wooden facades and decking. . International Research Group on Wood Protection, Stockholm, IRG/WP 09-20408.
Bornemann, T.; Brischke, C.; Lück, J.M. (2012) Comparative studies on the moisture performance and durability of wooden facades. Proceedings IRG annual meeting 2012. International Research Group on Wood Protection, Stockholm, IRG/WP 12-20492.
Humar, M.; Kržišnik, D.; Lesar, B.; Brischke, C. (2019) The performance of wood decking after five years of exposure: verification of the combined effect of wetting ability and durability. Forests. 10 [10], 903-920. https://doi.org/10.3390/f10100903
Niklewski, J.; Brischke, C.; Frühwald Hansson, E. (2021) Numerical study on the effects of macro climate and detailing on the relative decay hazard of Norway spruce. Wood Mater. Sci. Eng. 16 [1], 12-20. https://doi.org/10.1080/17480272.2019.1608296
Kutnik, M.; Montibus, M. (2019) Durability by design - a case study of the performance of wooden decks after 9.5 years of natural weathering. International Research Group on Wood Protection, Stockholm, IRG/WP 19-20648.
Niklewski, J.; Fredriksson, M. (2021) The effects of joints on the moisture behaviour of rain exposed wood: a numerical study with experimental validation. Wood Mater. Sci. Eng. 16 [1], 1-11. https://doi.org/10.1080/17480272.2019.1600163
Isaksson, T.; Thelandersson, S. (2013) Experimental investigation on the effect of detail design on wood moisture content in outdoor above ground applications. Build. Environ. 59, 239-249. https://doi.org/10.1016/j.buildenv.2012.08.023
Brischke, C.; Frühwald Hansson, E.; Kavurmaci, D.; Thelandersson, S. (2011) Decay hazard mapping for Europe. IRG/WP 11-20463. IRG, Stockholm.
Fruhwald Hansson, E.; Brischke, C.; Meyer, L.; Isaksson, T.; Thelandersson, S.; Kavurmaci, D. (2012) Durability of timber outdoor structures. Modelling performance and climatics impacts. In: World Conference on Timber Engineering. Auckland. 16-19.
Tajet, H.T.T.; Hygen, H.O. (2017) Potential risk of wood decay. MET report no. 8/2017 ISSN 2387-4201 Division for Climate Services. Norwegian Meteorological Institute.
Scheffer, T.C. (1971) A climate index for estimating potential for decay in wood structures above ground. Forest Prod. J. 21 [10], 25-31.
Fernández-Golfín Seco, J.I.; Peraza Sánchez, F.; Touza Vázquez, M.; Arriaga Martitegui, F. (2018) Guía para la asignación de clases de uso y de servicio a los productos de la madera. Monografía INIA Serie Forestal nº 30. España. Madrid. 95 pp. (in Spanish).
UNE EN 335:2013. Durability of wood and wood-based products - Use classes: definitions, application to solid wood and wood-based products (Spanish version). European Committee of Standardization (Spanish version).
PNE-prEN 460: 2020. Durability of wood and wood-based products - Natural durability of solid wood - Guide to the durability requirements for wood to be used in hazard classes.
Suttie, E.; Brischke, C.; Meyer, L.; Van Acker, J.; Kutnik, M.; Heisel, E.; Englund, F.; Jermer, J.; Thelandersson, S.; Polášek, M.; Lorenzo, D. (2014) Performance classification of wood in construction - drafting a user-friendly European standard. International Research Group on Wood Protection, Stockholm, IRG/WP 14-20545.
Kutnik, M.; Suttie, E.; Brischke, C. (2014) European standards on durability and performance of wood and wood-based products - Trends and challenges. Wood Mater. Sci. Eng. 9 [3], 122-133. https://doi.org/10.1080/17480272.2014.894574
Ministerio de Fomento (2009). Documento básico SE-M Seguridad estructural madera. Código Técnico de la Edificación (in Spanish).
Conde Garcia, M.; Conde García, M.; Fernández-Golfín, J.I. (2021) Improving the accuracy of wood moisture content estimation in four European softwoods from Spain. Forest Systems, 30 [1], e002. https://doi.org/10.5424/fs/2021301-17798
Conde García, M.; Conde García, M.; Fernández-Golfín, J.I. (2021) Species effect on decay resistance of wood exposed to exterior conditions above the ground in Spain. Mater. Construcc. 71 [341], e236. https://doi.org/10.3989/mc.2021.11320
Published
How to Cite
Issue
Section
License
Copyright (c) 2021 Consejo Superior de Investigaciones Científicas (CSIC)

This work is licensed under a Creative Commons Attribution 4.0 International License.
© CSIC. Manuscripts published in both the print and online versions of this journal are the property of the Consejo Superior de Investigaciones Científicas, and quoting this source is a requirement for any partial or full reproduction.
All contents of this electronic edition, except where otherwise noted, are distributed under a Creative Commons Attribution 4.0 International (CC BY 4.0) licence. You may read the basic information and the legal text of the licence. The indication of the CC BY 4.0 licence must be expressly stated in this way when necessary.
Self-archiving in repositories, personal webpages or similar, of any version other than the final version of the work produced by the publisher, is not allowed.
Funding data
Spanish National Plan for Scientific and Technical Research and Innovation
Grant numbers BIA2013-42434-R