Effect of MgO on compositions of the system CaO-Al2O3-Fe2O3. Solubility
DOI:
https://doi.org/10.3989/mc.1986.v36.i204.883Abstract
Five different compositions belonging to the equilibrium system CaO-Al2O3-Fe2O3 were dopep with a fixed quantity of MgO (6,5% wt). The compositions, which lie in different primary fields of crystallization and in different triangles of compatibility, were submitted to several thermal treatments. Each composition, which had previously been melted, originates in its solidification the aluminates and ferrites which are usual in the interstitial phase of clinker Portland, although they are in different microstructural arrangements. The effect of MgO on the generated microstructures has been shown. Also, the solubility of MgO on the aluminic and ferritic phases has been measured.
Downloads
Downloads
Published
How to Cite
Issue
Section
License
Copyright (c) 1986 Consejo Superior de Investigaciones Científicas (CSIC)

This work is licensed under a Creative Commons Attribution 4.0 International License.
© CSIC. Manuscripts published in both the print and online versions of this journal are the property of the Consejo Superior de Investigaciones Científicas, and quoting this source is a requirement for any partial or full reproduction.
All contents of this electronic edition, except where otherwise noted, are distributed under a Creative Commons Attribution 4.0 International (CC BY 4.0) licence. You may read here the basic information and the legal text of the licence. The indication of the CC BY 4.0 licence must be expressly stated in this way when necessary.
Self-archiving in repositories, personal webpages or similar, of any version other than the final version of the work produced by the publisher, is not allowed.